Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, MD = 0.130 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.130 GPa
18.9 ksi
ASTM D882
Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, Cast/Blown Film ResinCharacteristics: Good Drawdown, Can be used in blown or cast applicationsApplications:Stretch Wrap, CoextrusionsProcessing Conditions: Extruder 6.3..
Secant Modulus, MD 0.130 GPa
18.9 ksi
ASTM D882
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..
Secant Modulus, MD 0.130 GPa
18.9 ksi
ASTM D882
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim..
Secant Modulus, MD 0.130 GPa
18.9 ksi
ASTM D882
Huntsman PE 1402 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, MD 0.130 GPa
18.9 ksi
2% Secant; ASTM D882
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov..
Secant Modulus, MD 0.130 GPa
18.9 ksi
2% Secant Modulus; ASTM-D882
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene
CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE ..
Secant Modulus, MD 0.130 GPa
18.9 ksi
1%, Flexural; ASTM D882
Braskem Flexus® 9200 LLDPE Blown Film Extrusion
Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing ..
Copyright © lookpolymers.com All Rights Reserved