Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Polyolefin
Manufacturer Borealis
Trade Name Supersmooth™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acetate copolymer (EVA) and is designed to meet stringent shrinkback requirements for cables with aluminum conductors. It should not be used on copper conductors.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ASTM D1928/D 1505
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield >= 7.24 MPa
>= 1050 psi
Heat Aging (10 days at 135°C); ASTM D638
14.5 MPa
2100 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Tensile Set 100 %
100 %
Retention; ASTM D638
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 ohm-cm

@Temperature 23.0 °C
10.0 ohm-cm

@Temperature 73.4 °F
ASTM D991
1000 ohm-cm

@Temperature 90.0 °C
1000 ohm-cm

@Temperature 194 °F
ASTM D991
Processing Properties Metric English Comments
Melt Temperature 115 - 125 °C
239 - 257 °F
Drying Temperature 70.0 °C
158 °F