Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.22 MPa | 1050 psi | -5% change after 150 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N85U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 75-95 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade B1 (specification inactive for new design).Applications.. |
|||
Tensile Strength, Yield | 7.238 MPa | 1050 psi | -23% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S65E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specifica.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 513 Perfluoroelastomer Chemraz® 513 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contamination is required. This material offers excellen.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 517 Perfluoroelastomer Greene Tweed’s Chemraz® 517, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 517 has a Shore A.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 537 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance an.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7005 C TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | |
Spartech E65650 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | ASTM D-412-92 |
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture Features/Benefits:Outlasts silicone tubing in peristaltic pumps by up to 30 timesLow particulate spallationCan be autoclaved repeatedlyTemperature resistant from -60°F to 275°FWithstands repea.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3200-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-70-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | >= 7.24 MPa | >= 1050 psi | Heat Aging (10 days at 135°C); ASTM D638 |
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet.. |
|||
Tensile Strength, Yield | >= 7.24 MPa | >= 1050 psi | Heat Aging (168 hrs at 150°C); ASTM D638 |
Borealis Low Sulfur™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables Low Sulphur LE0594 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me.. |
|||
Tensile Strength, Yield | 7.24 MPa @Temperature 21.1 °C |
1050 psi @Temperature 70.0 °F |
Flatwise Tensile; Composite Honeycomb Sandwich Performance; ASTM C 297 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | ASTM D-638 |
Axiall 8553 Moldings & Extrusions Flexible PVC A general purpose profile extrusion compound with excellent weathering properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | ASTM D-638 |
Axiall 83-126J Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 7.24 MPa @Strain 300 % |
1050 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3880E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength, Yield | 7.24 MPa | 1050 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |