Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 ohm-cm @Temperature 90.0 °C |
1000 ohm-cm @Temperature 194 °F |
ASTM D991 |
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 500 °C |
<= 1000 ohm-cm @Temperature 932 °F |
|
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
|
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 25.0 °C |
<= 1000 ohm-cm @Temperature 77.0 °F |
|
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 500 °C |
<= 1000 ohm-cm @Temperature 932 °F |
|
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
|
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 25.0 °C |
<= 1000 ohm-cm @Temperature 77.0 °F |
|
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |