Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183-1 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183-1 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D792-91 |
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperat.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | Test Method A; ISO 1183:1987 |
Global EPP PA 6E Extruded Polyamide 6 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | |
Solvay AMPHIONIC® XL Surfactant Identification: AQUEOUS SOLUTION OF ALKYL AMINO POLYCARBOXYLATESAvailable in: Asia Pacific, Europe, Latin America and North America. Solubility: Readily soluble in water: in up to 35% NaOH and in.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis LE0592 Polyethylene LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D1928C/D 792 |
Borealis LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive LE0595-07 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. LE0595-07 is a crosslinkable black polyethylene compound, specially desi.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D1928/D 1505 |
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis Supersmooth™ LE0592S Polyethylene Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D792 |
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D792 |
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ASTM D792 |
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage .. |
|||
Density | 1.135 g/cc | 0.04100 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis Supersmooth™ LE8280 Polyethylene Insulation Compound, Crosslinkable Supersmooth™ LE8280 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE8280 is intended for semiconduct.. |