Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 10.0 ohm-cm @Temperature 900 °C |
10.0 ohm-cm @Temperature 1650 °F |
|
MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized Data provided by the supplier, MarkeTech International.8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are .. |
|||
Electrical Resistivity | 10.0 ohm-cm @Temperature 23.0 °C |
10.0 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet.. |