Material Notes:
Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and improved optical properties. Benefits can be obtained in terms of better down gauging possibilities and improved processability. Excellent printing quality is obtained due to high clarity and better layout.Himod FT7293 is intended for applications like: stiff films with excellent optical properties for automated packaging machinery, lamination film/food packaging, textile packaging films, and magazine packaging.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.929 g/cc
0.0336 lb/in³
ISO 1183
Thickness 40.0 microns
1.57 mil
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 550 ppm
550 ppm
Additive - Synthetic Silica
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ISO 527-3
Film Elongation at Break, TD 580 %
580 %
ISO 527-3
Secant Modulus, MD 0.230 GPa
33.4 ksi
ASTM D882-A
Secant Modulus, TD 0.260 GPa
37.7 ksi
ASTM D882-A
Impact 29
29
Puncture Resistance, force (N); ASTM D5748
Puncture Energy 0.400 J
0.295 ft-lb
ASTM D5748
Coefficient of Friction, Dynamic 0.40
0.40
ISO 8295
Tear Strength, Total 2.50 N
0.562 lb (f)
TD; ISO 6383/2
4.00 N
0.899 lb (f)
MD; ISO 6383/2
Dart Drop 2.00 g/micron
50.8 g/mil
ISO 7765/1
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ISO 527-3
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
ISO 11357/03
Vicat Softening Point 102 °C
216 °F
A (10N); ISO 306
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 110 %
110 %
ASTM D2457