Polymer Property : Dart Drop = 2.00 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.00 g/micron
50.8 g/mil
F<sub>50</sub>, ASTM D1709/A
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin
Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr..
Dart Drop 2.00 g/micron
50.8 g/mil
23°C; ASTM D1709
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Dart Drop 2.00 g/micron
50.8 g/mil
ASTM D1709
SABIC HP4023W Low Density Polyethylene for Blown Film
Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo..
Dart Drop 2.00 g/micron
50.8 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer.
Dart Drop 2.00 g/micron
50.8 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips MarFlex® 5355 LDPE Industrial Clarity, General Purpose Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Suited for High Speed Converting, Good Impact Strength, Excellent Processability, Good Sealability, Good OpenabilityApplications:Institutional Packaging, Food..
Dart Drop 2.00 g/micron
50.8 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 5455 LDPE Clear, General Purpose Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Good Clarity, High Gloss, Good Openability, Good Sealability, Suited for High Speed ConvertingApplications:Bakery and Food Products, Rack and Counter Merchand..
Dart Drop 2.00 g/micron
50.8 g/mil
38mm Dart, 66mm height; ASTM D1709
Reliance Industries Relene F46003 Polyethylene
Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu..
Dart Drop 2.00 g/micron
50.8 g/mil
F<sub>50</sub>, ASTM D1709/A
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin  (discontinued **)
Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at ..
Dart Drop 2.00 g/micron
50.8 g/mil
ASTM D1709
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene
LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
Dart Drop 2.00 g/micron
50.8 g/mil
ASTM D1709
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene
LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Dart Drop 2.00 g/micron
50.8 g/mil
ASTM D1709
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene
LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact ..
Dart Drop 2.00 g/micron
50.8 g/mil
ISO 7765/1
Borealis Himod™ FT7293 LDPE for Film
Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Dart Drop 2.00 g/micron
50.8 g/mil
ISO 7765/1
Borealis Himod™ FT7294 LDPE for Film
Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Dart Drop 2.00 g/micron
50.8 g/mil
ISO 7765/1
Borealis Himod™ FT7324 . LDPE for Film
Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Dart Drop 2.00 g/micron
50.8 g/mil
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food ..
Dart Drop 2.00 - 11.0 g/micron
50.8 - 279 g/mil
Average value: 3.48 g/micron Grade Count:24
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Dart Drop 2.00 g/micron
50.8 g/mil
23°C; ASTM D1709
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Dart Drop 2.00 g/micron
50.8 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer.
Dart Drop 2.00 g/micron
50.8 g/mil
ASTM D1709
SABIC HP2022 Series Low Density Polyethylene for Blown Film
Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:..