Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 40.0 - 150 microns | 1.57 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Thickness | 40.0 - 150 microns | 1.57 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |
|||
Thickness | 40.0 - 150 microns | 1.57 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Thickness | 40.0 - 150 microns | 1.57 - 5.91 mil | Recommended |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Thickness | 40.0 microns | 1.57 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 40 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
UBE 1022FDX29 Nylon 6 Homopolymer Film Specialties: Nucleated (Medium viscosity) Processing: T-die, Air blown Applications: General applications Information provided by UBE. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Borealis Borclear™ RB707CF Polypropylene Random Copolymer for Blown Film Borclear RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.Borclear RB707CF is especi.. |
|||
Thickness | 40.0 microns | 1.57 mil | for samples tested on this data sheet |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Thickness | 40.0 microns | 1.57 mil | for samples tested on this data sheet |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Thickness | 40.0 microns | 1.57 mil | for samples tested on this data sheet |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Thickness | 40.0 microns | 1.57 mil | for samples tested on this data sheet |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Borealis Borstar® FB4230 LLDPE for Film Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 526A Low Density Polyethylene, Blown Film Grade DOW LDPE 526A resin is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains medium levels of antiblock additive. .. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |
|||
Thickness | 40.0 microns | 1.57 mil | Adhesive Thickness |
Caplinq LINQTAPE™ PIT1A Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |
|||
Thickness | 40.0 microns | 1.57 mil | |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |