Physical Properties Metric English Comments
Thickness 40.0 - 150 microns
1.57 - 5.91 mil
Recommended
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability..
Thickness 40.0 microns
1.57 mil
± 2.5%; ASTM-252-78
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 40 µm)
PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap..
Thickness 40.0 - 80.0 microns
1.57 - 3.15 mil
Möller Medical PolySkin 98 S NanoCoating
Flexible, non-abrasive "soft feel" coating with velour-like surface.Information provided by Möller Medical, Member of CENTROTEC Group
Thickness 40.0 - 80.0 microns
1.57 - 3.15 mil
Indium Corp. NanoFoil® NF40 Nickel and Aluminum Localized Heat Source For Bonding
Features:40 microns thick - optimized for bonding electronics assembliesMinimum dimension 1.2mm x 2.0mmLocalized heat source for bondingEnables high-strength, high conductivity bonds between most co..
Thickness 40.0 microns
1.57 mil
UBE 1022FDX29 Nylon 6 Homopolymer Film
Specialties: Nucleated (Medium viscosity) Processing: T-die, Air blown Applications: General applications Information provided by UBE.
Thickness 40.0 microns
1.57 mil
Borealis Himod™ FT3280 LDPE for Film
Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Thickness 40.0 microns
1.57 mil
Borealis Himod™ FT5270 LDPE for Film
Himod FT5270 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Thickness 40.0 microns
1.57 mil
Borealis Himod™ FT7293 LDPE for Film
Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Thickness 40.0 microns
1.57 mil
Borealis Himod™ FT7294 LDPE for Film
Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Thickness 40.0 microns
1.57 mil
for samples tested on this data sheet
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt..
Thickness 40.0 microns
1.57 mil
for samples tested on this data sheet
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi..
Thickness 40.0 microns
1.57 mil
for samples tested on this data sheet
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch..
Thickness 40.0 microns
1.57 mil
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
Thickness 40.0 microns
1.57 mil
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..
Thickness 40.0 microns
1.57 mil
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film
Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure..
Thickness 40.0 microns
1.57 mil
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film
Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form ..
Thickness 40.0 microns
1.57 mil
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade
DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g..
Thickness 40.0 microns
1.57 mil
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade
DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con..
Thickness 40.0 microns
1.57 mil
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade
DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies..
Thickness 40.0 microns
1.57 mil
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..
Thickness 40.0 microns
1.57 mil
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..
Thickness 40.0 microns
1.57 mil
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an..
Thickness 40.0 microns
1.57 mil
Dow LDPE 682I Low Density Polyethylene, Film Grade
DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T..
Thickness 40.0 microns
1.57 mil
Adhesive Thickness
Caplinq LINQTAPE™ PIT2S
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Thickness 40.0 microns
1.57 mil
Adhesive Thickness
Caplinq LINQTAPE™ PIT1S
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Thickness 40.0 microns
1.57 mil
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion ..
Thickness 40.0 microns
1.57 mil
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..
Thickness 40.0 microns
1.57 mil
Dow LDPE 535I Low Density Polyethylene, Liner Grade
DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for..
Thickness 40.0 microns
1.57 mil
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..