Borealis Borstar® ME6052 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Borstar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borstar® ME6052 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borstar ME6052 is a black, bimodal, medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor-made properties important in jacketing applications, i.e. very low shrink back, excellent stress crack resistance and wide processing window. Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
Compound; ASTM D792
ESCR 10% Igepal® >= 2000 hour
>= 2000 hour
ASTM D1693/B
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield >= 24.8 MPa
>= 3600 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength >= 39.4 kV/mm
>= 1000 kV/in
At 20 mils; ASTM D149