LG Chemical DCPD

Category Fluid
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical DCPD.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Structure & Characteristics: Dimer of cyclopentadiene. Purified after Isolating from pyrolysis oil evolved during NCC pyrolysis processUses: Used during manufacturing of unsaturated polyester resin (UPR). The durability and physical properties of UPR had improved recently due to development of DCPD application technology.CAS: 77-73-6Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Vapor Pressure 0.0133 bar

@Temperature 48.0 °C
10.0 torr

@Temperature 118 °F
Vapor Density=4.6
Thermal Properties Metric English Comments
Boiling Point 172 °C
342 °F
Flash Point 32.0 °C
89.6 °F
Descriptive Properties Value Comments
Autoignition Temperature 503°C
Components C10’s
6-7%
C11’s
7-8%
DCPD
0.832
DICYCLOPETADIENE
0.832
TBC
23 ppm
TBC
23 ppm, ASTM D4590