Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 400 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Melt Flow | 0.70 g/10 min | 0.70 g/10 min | ASTM D1238 |
ExxonMobil OPTEMA™ TC 115 Blown Film Resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding
(discontinued **) Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 1.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Melt Flow | 0.70 g/10 min | 0.70 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Melt Flow | 0.70 g/10 min | 0.70 g/10 min | ASTM D1238 |
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound ApplicationsAQUATHENE FR 4098-00 is a colorable flame retardant masterbatch designed specifically for moisture cure applications. When FR 4098-00 is combined with AQ 120-000 and CM 04482 in the cor.. |
|||
Melt Flow | 0.70 - 0.85 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 - 0.85 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Borealis Borstar® ME6053 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar ME6053 is a natural, bimodal medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor made properties important in jacketing applications, .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis HE3366 High Density Polyethylene HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis HE4872 High Density Polyethylene HE4872 is a HDPE compound for solid insulation of symmetric data cable at high extrusion speed. Applications: high frequency data transmission cables, outer skin of foam-skin constructions. Specif.. |
|||
Melt Flow | 0.70 - 2.0 g/10 min | 0.70 - 2.0 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 470 Ethylene Vinyl Acetate DuPont™ Elvax® 470 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 470 resins can be used for the following applications: .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF1807 Low Density Polyethylene Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA .. |
|||
Melt Flow | 0.70 - 2.0 g/10 min | 0.70 - 2.0 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg |
0.70 g/10 min @Load 4.76 lb |
|
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Entec Hypel® PEHD.7/.962 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem EB 861 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Coextruded films; Shrink films for pallets; general purpose; mulching films. Information p.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem EB861/51 Blown Film Extrusion Low Density Polyethylene Film for general use; Shrink films; Coextrusion.Additives: Antiblock, DInformation provided by Braskem. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4007G Impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact.Applications: Suggested uses include profiles, tubing, squeeze bottles. UL temperature index of 100ºC.Process: Injection Mo.. |
|||
Melt Flow | 0.70 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.70 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa.. |