Material Notes:
BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination with LGF concentrates on the injection molding process. The product is available in natural color. Applications: BJ100HP has been developed especially for applications like: front end carriers, under body shieldings, door module carriers, dashboard carriers, and battery supports.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50mm/min; ISO 527-2
Elongation at Break 10 %
10 %
ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
1mm/min; ISO 527-2
Charpy Impact Unnotched 4.10 J/cm²

@Temperature -20.0 °C
19.5 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Processing Properties Metric English Comments
Middle Barrel Temperature 220 - 270 °C
428 - 518 °F
mass temperature
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F