Material Notes:
Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product meets FDA standards for food contact applications.Applications: Bottle blow molding, profile extrusion.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D-2240
Tensile Strength, Ultimate 22.1 MPa
3210 psi
2 in/min (50 mm/min); ASTM D638
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 520 %
520 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 14 %
14 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Descriptive Properties Value Comments
Process Blow Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved