Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7101 BLK Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO 1047-3000 COMPOUND The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 600 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Noble Polymers Ecobarrier™ 0512 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P.. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 8504 UV8D, 8504G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
Hyosung Topilene F300 PP F300 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R01A-00 Polypropylene Random Copolymer Random copolymer R01A-00 is an antistatic polypropylene produced by a unique catalyst technology. It is designed for blow molding and extrusion applications and exhibits good stiffness and improved .. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ISO 1133 |
Lucite International Diakon® TD735 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Techmer ES Statiblend® HIPS E AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and High Impact ResistanceAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® EA-0640 ABS, Unreinforced Permanent static prevention ABS material such as LCD carrierInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion Polypropylene PPR 3221 is a high clarity, high impact resistance random copolymer especially designed for blow molding applications (mono and multi-layers) for food and non-food packaging of sauces,.. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Melt Flow | 1.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
1.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock .. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | ASTM D1238 |
ExxonMobil Polybilt™ Bitumen Modifier 106 Low Density Polyethylene Resin Polybilt 106 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 106 content to achieve .. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem FF018F Homopolymer Polypropylene Description: Excellent Color and Processing Stability, Superior Optical and Mechanical Properties, Broad Processing WindowApplications: Suggested Uses Include BOPP ApplicationsThis resin meets the r.. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer The FP33 resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for film extrusion with good mechanical properties. It contains processing aid, slip, and.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
BASF Polystyrol® 168 NO Polystyrene (Europe) High molecular, heat-resistant grades for the extrusion of low-taint food packaging, especially BOPS.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Melt Flow | 1.8 g/10 min | 1.8 g/10 min | |
Kraton® D1102 + PP blend (50/50) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |