Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene Moplen EP300L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300L is a block copolymer selected by customers for use in in.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen RP370G Blow Molding Grade Polypropylene Moplen RP370G is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP370G is a copolymer particularly suitable for blow molding applicat.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ASTM D790 |
Flint Hills 13T25A Random Copolymer Polypropylene Features: Excellent clarity, blush resistant and good flexural modulus. Product does not contain animal derived components.Applications: Injection Molded - Lab ware, food packaging and medical. .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 8250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HD 7255 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 9450 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Sterigenics Raprex® R-100 Branched High Density Polyethylene Applications: ExtrusionRAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ISO 178 |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | |
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11 Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5021 Polypropylene, Blow Molding Grade Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product me.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3802 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Asia Technology Pioneers CAP 502 PP Nanocomposite Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3801 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3803 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ H5211PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |