Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F155 Epoxy Resin, T2C190 Carbon Tape

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F155 Epoxy Resin, T2C190 Carbon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: TXX190-12"-F155; Various fibersInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1518 MPa

@Temperature 24.0 °C
220200 psi

@Temperature 75.2 °F
1558 MPa

@Temperature 71.0 °C
226000 psi

@Temperature 160 °F
Tensile Modulus 117 GPa

@Temperature 71.0 °C
17000 ksi

@Temperature 160 °F
124.8 GPa

@Temperature 24.0 °C
18100 ksi

@Temperature 75.2 °F
Compressive Yield Strength 965 MPa

@Temperature 71.0 °C
140000 psi

@Temperature 160 °F
1172 MPa

@Temperature 24.0 °C
170000 psi

@Temperature 75.2 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.019
Laminate
Dry Resin Content (%) 38-40
Prepreg
Fiber Volume (%) 57
Laminate
Flow (%) 4-16
Copyright © lookpolymers.com All Rights Reserved