BLUESTAR 403HF-G20 PBT, 20% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer BLUESTAR
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BLUESTAR 403HF-G20 PBT, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ASTM D638
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Glow Wire Test 750 °C
1380 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Dielectric Strength 24.0 kV/mm
610 kV/in
ASTM D149