Polymer Property : Volume Resistivity = 2.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Celanese Celanex® 2016 PBT  (Unverified Data**)
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese Celanex® XFR 6842 GF30 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex XFR 6842 GF30 is a halogen and antimony free flame retardant (V-0 @ 0.4 mm) 30% glass reinforced PBT grade with good processability and no corrosive emissions during processing. It is suita..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Volume Resistivity 2.00e+16 ohm-cm

@Temperature 23.0 °C
2.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)  (Unverified Data**)
Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese VECTRA FIT70 LCP, 35% Mineral / Glass Reinforced  (Unverified Data**)
35% glass and mineral reinforced grade. It offers excellent flowability, low warpage, excellent surface appearance, excellent dimensional stability, and good weldline strength. 35% glass/ mineral re..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PP G/CF40 CC 40% Glass/Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
GB/T1410-2006
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Volume Resistivity >= 2.00e+16 ohm-cm
>= 2.00e+16 ohm-cm
IEC 60093
Styrolution Novodur® M205FC ABS
Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PC GF20 X 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Mold ReleaseFeatures: Good Mold Release and High FlowInformation provided by T..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Polyplastics Duranex® 313RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
50% RH; ASTM D257
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
50% RH; tested on 10 mil thickness sample; ASTM D257
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
50% RH; tested on 10 mil thickness sample; ASTM D257
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
50% RH; tested on 10 mil thickness sample; ASTM D257
DuPont™ Nomex® 410 Paper, 30 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese CELANEX 4202 PBT, 15% Glass Reinforced
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.Information provided by Celanese
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese VECTRA FIT70 LCP, 35% Mineral / Glass Reinforced
35% glass and mineral reinforced grade. It offers excellent flowability, low warpage, excellent surface appearance, excellent dimensional stability, and good weldline strength.Information provided b..
Volume Resistivity 2.00e+16 ohm-cm

@Thickness 2.00 mm
2.00e+16 ohm-cm

@Thickness 0.0787 in
ASTM D257
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.Information provided by Celanese
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
IEC 60093
Celanese CELANEX XFR 6842 GF30 PBT, 30% Glass Reinforced
Celanex XFR 6842 GF30 is a halogen and antimony free flame retardant (V-0 @ 0.4 mm) 30% glass reinforced PBT grade with good processability and no corrosive emissions during processing. It is suita..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Celanese CoolPoly® D8102 Thermally Conductive Thermoplastic Elastomer
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
BLUESTAR 403HF-G30 PBT, 30% Glass Filled
Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS).
Volume Resistivity 2.00e+16 ohm-cm

@Temperature 23.0 °C
2.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Volume Resistivity 2.00e+16 ohm-cm

@Temperature 23.0 °C
2.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced
Celanex 3116 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), 7.5% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla..