Material Notes:
Description: Ultramid® C33 LN is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion with temperature sensitive polymers like EVOH Product supplied in 2-2.5 mm round pellets.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
Density 1.12 g/cc
0.0405 lb/in³
Water Absorption 10.5 %
10.5 %
saturation in water 23°C
Moisture Absorption at Equilibrium 3.2 %
3.2 %
23°C/50% RH
Water Vapor Transmission 50.0 g/m²/day
3.22 g/100 in²/day
85% RH
Oxygen Transmission Rate 21.0 cc/m²/day
1.35 cc/100 in²/day
50% RH
Viscosity Measurement 3.19 - 3.41
3.19 - 3.41
(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
187 - 203
187 - 203
(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
TD
80.0 MPa
11600 psi
MD
Elongation at Break 450 %
450 %
TD
450 %
450 %
MD
Tensile Modulus 1.40 GPa
203 ksi
MD
Thermal Properties Metric English Comments
Melting Point 195 - 197 °C
383 - 387 °F
ISO 3146
Decomposition Temperature >= 300 °C
>= 572 °F
Processing Properties Metric English Comments
Moisture Content 0.080 %
0.080 %
ISO 15512
Descriptive Properties Value Comments
Commercial Status Europe
Extractables <0.8 %
ISO 6427
Film Grade 1-3
BASF
Ignition Temperature >400°C
ASTM D1929
Lubricant 250 - 550 mg/kg
BASF
Nucleating Agent 250 - 550 mg/kg
BASF