Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 300 °C | 572 °F | 1% mass loss, N2; TGA |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® A24 E 01 PA66 Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B40 L PA6 Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round .. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B40 LN PA6 Description: Ultramid® B40 LN is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film. Clarity and thermoformability are enhanced by the incorporation.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C31 01 PA6/66 Description: Ultramid® C31 01 is a copolyamide 6/66 grade of low viscosity that is well suited for the production of compounds and blends. Product supplied in 2-2.5 mm CYLINDRICAL pellets.Informati.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C33 L PA6/66 Description: Ultramid® C33 L is a lubricated copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Ultramid® C33 L is well suited for the production of nonsymmetr.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C33 LN 0.025 mm Blown Film PA6/66 Description: Ultramid® C33 LN is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C40 L 01 PA6/66 Description: Ultramid® C40 L 01 is a lubricated copolyamide 6/66 grade of high viscosity for the production of monofilaments and blown film. Ultramid® C40 L 01 is well suited for the production of.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C40 LN 01 PA6/66 Description: Ultramid® C40 LN 01 is a copolyamide 6/66 grade of high viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion with.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B27 SD 02 PA6 Description: Ultramid® B27 SD 02 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B33 L PA6 Description: Ultramid® B33 L is a lubricated polyamide 6 grade of intermediate viscosity that is well suited for the production of biaxial oriented and cast film and monofilaments. Product comes .. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B36 PA6 Description: Ultramid® B36 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film and monofilaments. Product comes in 2-2.5 mm round .. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B36 LN 01 PA6 Description: Ultramid® B36 LN 01 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film. Clarity and thermoformability are enhanced b.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |