Polymer Property : Bulk Density = 0.710 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C31 01 PA6/66
Description: Ultramid® C31 01 is a copolyamide 6/66 grade of low viscosity that is well suited for the production of compounds and blends. Product supplied in 2-2.5 mm CYLINDRICAL pellets.Informati..
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C33 L PA6/66
Description: Ultramid® C33 L is a lubricated copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Ultramid® C33 L is well suited for the production of nonsymmetr..
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C33 LN 0.025 mm Blown Film PA6/66
Description: Ultramid® C33 LN is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion..
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C40 L 01 PA6/66
Description: Ultramid® C40 L 01 is a lubricated copolyamide 6/66 grade of high viscosity for the production of monofilaments and blown film. Ultramid® C40 L 01 is well suited for the production of..
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C40 LN 01 PA6/66
Description: Ultramid® C40 LN 01 is a copolyamide 6/66 grade of high viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion with..
Bulk Density 0.690 - 0.710 g/cc
0.0249 - 0.0257 lb/in³
BASF Ultramid® C33 PA6/66
Description: Ultramid® C33 is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film and monofilaments. Ultramid® C33 is well suited for the production of nonsymm..