BASF Pluracol® 2086 Slabstock Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 2086 Slabstock Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF
Physical Properties Metric English Comments
Density 0.989 g/cc

@Temperature 54.5 °C
0.0357 lb/in³

@Temperature 130 °F
1.01 g/cc

@Temperature 32.2 °C
0.0365 lb/in³

@Temperature 90.0 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 110 cP

@Temperature 54.5 °C
110 cP

@Temperature 130 °F
340 cP

@Temperature 32.2 °C
340 cP

@Temperature 90.0 °F
503 cP

@Temperature 25.0 °C
503 cP

@Temperature 77.0 °F
Molecular Weight 2800 g/mol
2800 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <50
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 56 - 59.2 mg KOH/g
STI 3007/3162
Unsaturation <0.05 meq/g
STI 3056