Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 340 cP @Temperature 32.2 °C |
340 cP @Temperature 90.0 °F |
|
BASF Pluracol® 2086 Slabstock Foam Polyol Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF |