Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.989 g/cc @Temperature 54.5 °C |
0.0357 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 1538 Slabstock Foam Polyol Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immi.. |
|||
Density | 0.989 g/cc @Temperature 54.5 °C |
0.0357 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 2086 Slabstock Foam Polyol Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF |
|||
Density | 0.989 g/cc @Temperature 60.0 °C |
0.0357 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 2100 Slabstock HR Foam Polyol Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Plurac.. |
|||
Density | 0.989 g/cc @Temperature 60.0 °C |
0.0357 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 380 Specialty Polyol Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation.. |