Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.987 g/cc @Temperature 37.8 °C |
0.0357 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® 1044 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 0.989 g/cc @Temperature 54.5 °C |
0.0357 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 1538 Slabstock Foam Polyol Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immi.. |
|||
Density | 0.989 g/cc @Temperature 54.5 °C |
0.0357 lb/in³ @Temperature 130 °F |
|
BASF Pluracol® 2086 Slabstock Foam Polyol Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF |
|||
Density | 0.989 g/cc @Temperature 60.0 °C |
0.0357 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 2100 Slabstock HR Foam Polyol Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Plurac.. |
|||
Density | 0.989 g/cc @Temperature 60.0 °C |
0.0357 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 380 Specialty Polyol Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation.. |
|||
Density | 0.987 g/cc @Temperature 60.0 °C |
0.0357 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® TP 4542 Specialty Polyol Description: Pluracol® TPE 4542 polyol is a moderately high molecular weight polyether triol that can be used in polyurethane sealant applications, flexible integral skin foam and cold-cured foam a.. |