Polymer Property : Viscosity = 110 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 110 cP

@Shear Rate 1000 1/s,
Temperature 250 °C
110 cP

@Shear Rate 1000 1/s,
Temperature 482 °F
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY
Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i..
Viscosity 110 cP

@Temperature 54.5 °C
110 cP

@Temperature 130 °F
BASF Pluracol® 2086 Slabstock Foam Polyol
Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF
Viscosity 110 cP

@Temperature 60.0 °C
110 cP

@Temperature 140 °F
BASF Pluracol® 726 Specialty Polyol
Description: Pluracol® 726 polyol is a 3000 molecular weight propylene oxide adduct of glycerine. Originally designed as a slabstock foam polyol, Pluracol 726 has found wide acceptance in specialty..
Viscosity 110 cP

@Shear Rate 1000 1/s,
Temperature 300 °C
110 cP

@Shear Rate 1000 1/s,
Temperature 572 °F
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..