Polymer Property : Molecular Weight = 2800 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 2800 g/mol
2800 g/mol
C.O.I.M. DIEXTER® G170 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 2800 g/mol
2800 g/mol
C.O.I.M. DIEXTER® G216 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 2800 g/mol
2800 g/mol
C.O.I.M. DIEXTER® G240 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 2800 g/mol
2800 g/mol
BASF Pluracol® 2086 Slabstock Foam Polyol
Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF
Molecular Weight 2800 g/mol
2800 g/mol
C.O.I.M. DIEXTER® G172 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Molecular Weight 2800 g/mol
2800 g/mol
Solvay Specialty Polymers FOMBLIN® Y H-VAC 18/8 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..