Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility at low temperatures - Good weathering properties - Non-halogen flame retardant - Glossy/Transparent - EEC Food Contact Approved - FDA Food Contact Approved - NSF 61 Portable Water Approved - USP Medical Class VIApplications: - Energy & Power Cables: coiled or spiral: Construction / Mining - Automotive Cables: Anti-lock Braking Systems – ABS - Industrial Cables: Traffic / Signal / Trains / Boats / Buildings - Geophysical Cables: Land & Off-shore; Marine, Sub-sea & Umbilical - Telecommunications Cables: Telephone & Data Transmission; Military and Fiber Optics - Audio and Medical CablesInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength 55.2 MPa
8000 psi
ASTM D412
Tensile Strength, Yield 10.3 MPa

@Strain 50.0 %
1500 psi

@Strain 50.0 %
ASTM D412
13.1 MPa

@Strain 100 %
1900 psi

@Strain 100 %
ASTM D412
29.0 MPa

@Strain 300 %
4200 psi

@Strain 300 %
ASTM D412
Elongation at Break 530 %
530 %
ASTM D412
Tear Strength 628 kN/m
3580 pli
ASTM D624
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Flammability, UL94 V-2

@Thickness 2.00 mm
V-2

@Thickness 0.0787 in
V-2

@Thickness 6.00 mm
V-2

@Thickness 0.236 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Abrasion Loss (mm3) 35
DIN 53516