BASF Elastollan SP 852 TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan SP 852 TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance. Typical Applications: Polyester based easy flow.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
ISO 868
Tensile Strength 2.30 MPa
334 psi
20; ISO 37
5.00 MPa
725 psi
100; ISO 37
8.50 MPa
1230 psi
300; ISO 37
50.0 MPa
7250 psi
ISO 37
Elongation at Break 680 %
680 %
ISO 37
Charpy Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DIN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN ISO 179
Tear Strength 70.0 kN/m
399 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 23 %

@Temperature 23.0 °C
23 %

@Temperature 73.4 °F
DIN EN ISO 815
42 %

@Temperature 70.0 °C
42 %

@Temperature 158 °F
DIN EN ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
175 - 240 °C
347 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion