Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 334 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 2.30 MPa
334 psi
20; ISO 37
BASF Elastollan SP 852 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 2.30 MPa
334 psi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Copyright © lookpolymers.com All Rights Reserved