Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.50 MPa | 1230 psi | ISO 37 |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE COPEC® CC6FDN Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS The VS/MR/AD1 Series is recommended for applications in the consumer electronics section. The series features an exceptionally silky and velvety surface, accompanied by an outstanding resistance to .. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® K TC8PCN Thermoplastic Elastomer, Adhesion to PA, optimized compression set The AD/PA/CS Series is recommended for applications with excellent adhesion to PA as well as outstanding compression set. The compounds are available in natural and black colors. Typical application.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® K TP7NLB Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA The AD2 Series is recommended for applications with excellent adhesion to polar thermoplastics such as SAN, ASA, PMMA. The compounds are available in natural and black colors. Typical applications: .. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® K TP7NLZ Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA The AD2 Series is recommended for applications with excellent adhesion to polar thermoplastics such as SAN, ASA, PMMA. The compounds are available in natural and black colors. Typical applications: .. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® M TM5MHD Thermoplastic Elastomer, for medical and pharmaceutical technology The MC/n Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The compounds are produced exclusively by a special med.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® K TC6GPN Thermoplastic Elastomer, General purpose The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | |
Momentive Performance Materials FQE207U Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-30AB Elastomer KE-2090-30 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | 300; ISO 37 |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 8.50 MPa | 1230 psi | DIN 53504/ISO 37 |
Kraiburg TPE THERMOLAST® K TP5LDZ Thermoplastic Elastomer, Low Density, Automotive Exterior Applications The UV/LD/b Series is recommended for applications requiring high UV resistance. It is particularly appropriate for automotive exterior. Typical applications: Cowls gasketsRoof rimsWater deflectorsW.. |