Material Notes:
Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are greatly reduced.Trenchless solutions can be implemented quicker than traditional construction techniques.Risk to public during the construction process is greatly minimized.Road surfaces do not have to be replaced.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D-785
Hardness, Shore D 73.8
73.8
ASTM D-2240
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D-638
Tensile Modulus 1.54 GPa
223 ksi
ASTM D-638
Flexural Strength 40.9 MPa
5930 psi
ASTM D-790
Flexural Modulus 0.5510 GPa
79.92 ksi
ASTM D-790
Izod Impact, Notched 11.1 J/cm

@Thickness 6.35 mm
20.8 ft-lb/in

@Thickness 0.250 in
ASTM D-256
12.7 J/cm

@Thickness 3.17 mm
23.8 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.00 °C
123.8 °F
annealed; ASTM D-648