Polymer Property : Izod Impact, Notched = 23.8 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 12.7 J/cm

@Thickness 3.17 mm
23.8 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall Vynaprene 7907 Rigid PVC, Extrusion
Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre..