Deflection Temperature at 1.8 MPa (264 psi) 51.00 °C
123.8 °F
annealed; ASTM D-648
Axiall Vynaprene 7907 Rigid PVC, Extrusion
Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre..