Mechanical Properties Metric English Comments
Flexural Strength 40.9 MPa
5930 psi
ASTM D-790
Axiall Vynaprene 7907 Rigid PVC, Extrusion
Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre..