Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.54 GPa | 223 ksi | 1mm/min |
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 1.54 GPa | 223 ksi | |
Abatron AboCast 8103-24 High-Performance Dielectric Epoxy AboCast 8103-24 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has an exc.. |
|||
Tensile Modulus | 1.54 GPa | 223 ksi | ASTM D-638 |
Axiall Vynaprene 7907 Rigid PVC, Extrusion Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre.. |