Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.7 J/cm @Thickness 3.17 mm |
23.8 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall Vynaprene 7907 Rigid PVC, Extrusion Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre.. |