Polymer Property : Tensile Strength, Yield = 27.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D882
Formosa Plastics Formolene® LH5320 Injection Molding HDPE  (discontinued **)
CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5320 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm..
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D882
Formosa Plastics Formolene® LH5326 Injection Molding HDPE  (discontinued **)
CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm..
Tensile Strength, Yield 27.1 MPa
3930 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 27.1 MPa
3930 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D638
Entec Hypel® PEHD20/.953 HDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Tensile Strength, Yield 27.1 MPa
3930 psi
2.0 in/min; ASTM D638
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D638
Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene
HDPE 175953 features easy flow, toughness, and high surface gloss. Applications include caps, thin wall parts, and toys.Former A-Top Polymers product; part of Amco product line since 2013.
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D-638
Axiall Vynaprene 7907 Rigid PVC, Extrusion
Georgia Gulf 7907 is a rigid compound designed for the trenchless rehabilitation of decaying sewer pipes. Advantages include: Cost & time required for the construction phase of the project are gre..
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D882
Formosa Plastics Formolene® LH5212 Injection Molding HDPE  (discontinued **)
CopolymerApplications: Pails, buckets, housewares, cartridges, closures, toysFormolene LH5212 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Foo..
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D638
Formosa Plastics Formolene® LH5214 Injection Molding HDPE  (discontinued **)
High Density Polyethylene for Injection Molding Applications Formolene® LH5214 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of ..