Polymer Property : Izod Impact, Notched = 22.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 11.7 J/cm

@Thickness 3.17 mm
22.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9113 Rigid PVC, Molding
Georgia Gulf 9113 is used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. It has excellent impact strength.Information provided by Georgia GulfGeorgi..
Izod Impact, Notched 11.7 J/cm

@Thickness 3.17 mm
22.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9113J Clear 13, 9113J Clear 61 Rigid PVC, Molding, Clear 13, Clear 61
Georgia Gulf 9113J Clear 13 and 9113J Clear 61 are used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. They have excellent impact strength and conta..
Izod Impact, Notched 11.7 J/cm

@Thickness 3.17 mm
22.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 9113 White 02 Rigid PVC, Molding, White 02
Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi..