Material Notes:
Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: PelletsProcessing Method: Extrusion and Injection MoldingAfrica & Middle EastAsia PacificEuropeLatin AmericaNorth AmericaSouth America
Physical Properties Metric English Comments
Density 0.700 g/cc
0.0253 lb/in³
Apparent; ASTM D1182
1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
Equilibrium; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85

@Thickness 6.35 mm
85

@Thickness 0.250 in
ASTM D785
Tensile Strength, Yield 66.9 MPa

@Thickness 3.18 mm
9700 psi

@Thickness 0.125 in
6 mm/min; ASTM D638
Elongation at Break 5.0 %

@Thickness 3.18 mm
5.0 %

@Thickness 0.125 in
6 mm/min; ASTM D638
Flexural Strength 97.9 MPa

@Thickness 6.35 mm
14200 psi

@Thickness 0.250 in
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.200 J/cm

@Thickness 6.35 mm
0.375 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C

@Thickness 6.35 mm
198 °F

@Thickness 0.250 in
unannealed; ASTM D648
Vicat Softening Point 105 °C
221 °F
50°C/hr; ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
UL 94
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Transmission, Visible 92 %

@Thickness 3.18 mm
92 %

@Thickness 0.125 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.7
3.7
ASTM D150
Dielectric Strength 0.787 kV/mm
20.0 kV/in
ASTM D149
Dissipation Factor 0.19
0.19
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 185 - 200 °C
365 - 392 °F
Middle Barrel Temperature 210 - 225 °C
410 - 437 °F
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 75.0 - 80.0 °C

@Time 14400 sec
167 - 176 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Power Factor 0.5
ASTM D150