Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1231 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
MRC Polymers NAXALOYâ„¢ 770-NT137 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1702 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PET IM 1016 UV Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/66 IM3 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection Moldi.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 6.35 mm |
12.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9113 White 02 Rigid PVC, Molding, White 02 Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |