Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.1 MPa | 6110 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.1 MPa | 6110 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.1 MPa | 6110 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6110 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6110 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Global ABS-0305 General Purpose ABS
(discontinued **) Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Global ABS-308 Easy Flow, General Purpose ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Global ABS-406 General Purpose ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM-D638 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Spartech Royalite R47 PVC Alloy Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D882 |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Techmer ES Statiblend® ABS AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 42.1 MPa @Thickness 3.17 mm |
6110 psi @Thickness 0.125 in |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM 638 |
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by We.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Westlake Plastics Tefzel® 2181 ETFE Products made from Tefzel® HT-2181 resin are suitable for a variety of processes and demanding end uses. They are mechanically tough and offer an excellent balance of properties. These products p.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Total PSC 500 Polystyrene Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in pro.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7600B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D638 |
Dow INSPIRE™ 404 Performance Polymer INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of t.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D-638 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |
|||
Tensile Strength, Yield | 42.1 MPa | 6110 psi | ASTM D638 |
Braskem INSPIRE™ 404 Performance Polypropylene Polymer INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of .. |
|||
Tensile Strength, Yield | 42.1 MPa | 6100 psi | ASTM D-638 |
Axiall 9113 White 02 Rigid PVC, Molding, White 02 Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi.. |