Material Notes:
AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other optical components. AA-BOND F113 is recommended for laminating, bonding, and sealing applications where excellent wetting, good pot life and improved impact strength properties are required. AA-BOND F113 is two parts adhesive easily mixed and cured at room temperature and develops strong bond to glass and glass fibers, ceramics, many metals and most rigid plastics. AA-BOND F113 bonds offer resistance to mechanical impact and thermal shock, and is also resistant to weather, water, gases and vapors, petroleum products, and mild acids and alkalis. Appearance: ClearCure Type: Heat cure or Room TemperatureBenefits:Low viscosityThermal shock and impact resistantLow stress connections Mix Ratio by weight: 100:30/Resin:Hardener Typical Application: Fiber optic assembly, multimode and single mode connectors, small potting and sealing applicationsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
uncured
Water Absorption at Saturation 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
cured
Viscosity 175 cP
175 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Adhesive Bond Strength 27.6 MPa

@Temperature 65.0 °C,
Time 7200 sec
4000 psi

@Temperature 149 °F,
Time 2.00 hour
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C
34.4 µin/in-°F
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 45.0 °C
113 °F
Optical Properties Metric English Comments
Refractive Index 1.51
1.51
cured
Transmission, Visible 97 %
97 %
cured
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+8 ohm-cm
9.00e+8 ohm-cm
Dielectric Constant 4.8

@Frequency 1000 Hz
4.8

@Frequency 1000 Hz
Dielectric Strength 16.9 kV/mm
430 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 65.0 °C
1.00 - 2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 2.00 min
2.00 min
uncured
Descriptive Properties Value Comments
Thixotropic Index 1