Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
S&E Specialty Polymers TufGuard E™ GTPO8102ROHS Olefin-based, Flame Retardant Application: The GTPO8102ROHS compound is an FR, UV, olefin-based insulation and jacketing compound for appliance, flat ribbon and heat trace wire applications. It is formulated to meet CSA test C22.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D 792 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Kolon KOPA® KN333C22 CF Reinforced Nylon 66 Carbon 22%, high strengthApplications Cylinder piston partsInformation provided by API-Kolon. |
|||
Specific Gravity | 1.23 - 1.29 g/cc | 1.23 - 1.29 g/cc | ASTM D 792 |
Karina 601D10/1-A White PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.27 g/cc | 1.23 - 1.27 g/cc | ASTM D 792 |
Karina 75/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 - 1.27 g/cc | 1.23 - 1.27 g/cc | ASTM D 792 |
Karina 75/202 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ISO 1183 |
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Specific Gravity | 1.23 g/cc @Temperature 25.0 °C |
1.23 g/cc @Temperature 77.0 °F |
|
Multibase Dow Corning® MB40-006 Siloxane Additive DOW CORNING MB40-006 Masterbatch is a pelletized formulation containing 40% of an ultra-high molecular weight siloxane polymer dispersed in POM polymer. It is designed to be used as an additive in P.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D297, 15 |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | +.02 |
Spartech E66091 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Specific Gravity | 1.23 g/cc @Temperature 22.8 °C |
1.23 g/cc @Temperature 73.0 °F |
ASTM D792 |
Spartech PP5440 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® RCX201 PC+PET (Asia Pacific) |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 90-A41R-80-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SGH 6500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL GFN2L PPE+PS (Asia Pacific) PPE+PS GF20%, hydrolytic stability |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | |
Shin-Etsu Silicones KE-5540U Low Temperature Silicone Elastomer ShinEtsu KE5540 U is a nominal 40 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Teknor Apex APEX® 90-A471R-85-NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Chase Plastics CP Pryme® N313GL (COND, 50% RH) Nylon 6 (Utility Grade), 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Red 5670 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5670 is a red color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 56.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D7920-66 |
DuPont Performance Polymers Neoprene GNA Polychloroprene DuPont™ Neoprene GNA is a sulfur-modified polychloroprene stabilized with a thiuram disulfide and a staining antioxidant. It should not be used in applications where resistance to staining or disco.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D-792 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Specific Gravity | 1.23 - 1.27 g/cc | 1.23 - 1.27 g/cc | ASTM D-792 |
Axiall 113B-FR Moldings & Extrusions Flexible PVC Non-lead stabilized, 105°C rated injection molding compound. Rated 94 V-0 at 1.5 mm and 94 V-1 at 0.58 mm for all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |
|||
Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |