Material Notes:
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy processes. A low coefficient of thermal expansion, good thermal conductivity and good material properties at elevated temperatures combine for superior performance in a variety of applications. This unusual combination of properties results in less thermal fatigue and soldering in the die cast or extrusionApplications:Die Cast ToolingExtrusion DiesHot Runner NozzlesVibration and Tool Chatter ReductionPlastic Injection MoldingHigh Elongation RequirementsMaximum Thermal Conductivity NeedsShot SleevesAstaras, Inc. purchased the entire Anviloy® business from CMW in 2014. Information provided by Astaras, Inc.
Physical Properties Metric English Comments
Density 17.25 g/cc
0.6232 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 34
34
Hardness, Vickers 335
335
HV10
Tensile Strength, Ultimate 517 MPa

@Temperature 816 °C
75000 psi

@Temperature 1500 °F
724 MPa

@Temperature 649 °C
105000 psi

@Temperature 1200 °F
779 MPa

@Temperature 538 °C
113000 psi

@Temperature 1000 °F
950 MPa

@Temperature 22.2 °C
138000 psi

@Temperature 72.0 °F
Tensile Strength, Yield 650 MPa
94300 psi
Elongation at Break >= 10 %
>= 10 %
in 2 in (51 mm)
Modulus of Elasticity 338 GPa
49000 ksi
Flexural Modulus 1.52 GPa
220 ksi
Thermal Properties Metric English Comments
CTE, linear 4.53 µm/m-°C

@Temperature 20.0 - 400 °C
2.52 µin/in-°F

@Temperature 68.0 - 752 °F
5.26 µm/m-°C

@Temperature 20.0 - 800 °C
2.92 µin/in-°F

@Temperature 68.0 - 1470 °F
Thermal Conductivity 70.2 W/m-K
487 BTU-in/hr-ft²-°F
Melting Point 1425 - 3410 °C
2597 - 6170 °F
Solidus 1425 °C
2597 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Iron, Fe 2.0 %
2.0 %
Molybdenum, Mo 4.0 %
4.0 %
Nickel, Ni 4.0 %
4.0 %
Tungsten, W 90 %
90 %
Users viewing this material also viewed the following: