Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 517 MPa

@Temperature 816 °C
75000 psi

@Temperature 1500 °F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Tensile Strength, Ultimate 517 MPa

@Temperature 816 °C
75000 psi

@Temperature 1500 °F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..