Polymer Property : Melting Point = 1425 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1425 - 3410 °C
2597 - 6170 °F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Melting Point 1425 - 3410 °C
2597 - 6170 °F
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Melting Point 1425 - 3410 °C
2597 - 6170 °F
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Melting Point 1425 °C
2597 °F
California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1425 °C
2597 °F
California Fine Wire NIFE 5200 Nickel Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Melting Point 1425 - 3410 °C
2597 - 6170 °F
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Melting Point 1425 - 1510 °C
2597 - 2750 °F
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..