Density 17.25 g/cc
0.6232 lb/in³
MarkeTech 91-6-3 Tungsten Alloy, AMS-T-21014 Class 1
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
Density 17.25 g/cc
0.6232 lb/in³
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..
Density 17.25 g/cc
0.6232 lb/in³
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr..